Mode II fracture-parameter estimates for concrete from beam specimens
SE Swartz, LW Lu, LD Tang, TME Refai - Experimental Mechanics, 1988 - Springer
... The load was applied by moving the piston/support assembly/test specimen/ spreader
beam upward to make contact with the load ... K32 102 0.29 524 33 40 13.4 1294 L ...
Hydrometallurgical process for recovery of metal values from spent lithium-ion secondary batteries -
P Zhang, T Yokoyama, O Itabashi, TM Suzuki, K … - Hydrometallurgy, 1998 - Elsevier
... tube or a 500 ml separatory funnel at ambient temperature ( 25?C). A contact time
of 30 ... 0.29 M D2EHPA 2.2:1 6.71 7.1 x 102 0.29 M D2EHPA 2.2:1 7.17 6.5 ? 102 ...
Effect of 0.29% w/w fipronil spray on adult flea mortality and egg production of three different cat … -
PA Payne, MW Dryden, V Smith, RK Ridley - Veterinary Parasitology, 2001 - Elsevier
... 6 ml/kg of Frontline ? spray (0.29% w/w ... Corresponding Author Contact Information
Corresponding author ... Veterinary Parasitology Volume 102, Issue 4, 28 December ...
Molecular dynamics of Poiseuille flow and moving contact lines -
J Koplik, JR Banavar, JF Willemsen - Physical Review Letters, 1988 - APS
... the viscous dissipation diverges logarith- mically at the contact line.3 ... m DiiT/a2
0 o.. 7.47X 102 0.025 1.85 0.5 0.13 0.05 2.05 ? 0.5 0.29 ? 0.03 0.075 ...
Dating mafic-ultramafic intrusions by ion-microprobing contact-melt zircon: examples from SW Sweden -
A Scherst?n, H ?reb?ck, D Cornell, P Hoskin, A … - Contributions to Mineralogy and Petrology, 2000 - Springer
... HAS 96002 Hakefjorden Complex contact migmatite ... 25.4 1944 242 569 0.29 354 0.0764
4.97 0.1211 6.77 1.275 8.94 ... 0.0996 0.50 0.2918 1.44 4.007 1.57 0.95 102 1616 8 ...
Experimental and theoretical investigation of a capillary pumped loop with a porous element in the … -
I Muraoka, FM Ramos, VV Vlassov - International Communications in Heat and Mass Transfer, 1998 - Elsevier
... of the bubble is in contact with the wick and the other half is in contact with
the ... 120 W / 40 ?C exp theo 76.7 79.2 67.5 70.3 67.4 69.7 36.7 39.2 102 0.29 ...
Knee cartilage topography, thickness, and contact areas from MRI: in-vitro calibration and in-vivo … -
ZA Cohen, DM McCarthy, SD Kwak, P Legrand, F … - Osteoarthritis and Cartilage, 1999 - Elsevier
... followed by the femur (0.33 mm and 0.29 mm respectively ... 6. Patellar contact area
from MRI of a cadaver knee ... 102 Cohen et al.: Cartilage quantification from MRI ...
Contact order, transition state placement and the refolding rates of single domain proteins -
KW Plaxco, KT Simons, D Baker - Journal of Molecular Biology, 1998 - Elsevier
... are related to the relative contact order of the native state, the correlation between
? m and refolding rates is relatively poor (r = 0.34, p = 0.29). ...
Electrical activity, mode of incorporation and distribution coefficient of group V elements in Hg 1 … -
HR Vydyanath, JA Ellsworth, CM Devaney - Journal of Electronic Materials, 1987 - Springer
... of Hg and z' moles of Te at a temperature above T and quenching it to room
temperature--is brought in contact with CdTe at ... 102 0.29 P, 0.3 3 ? 1016 p type 332 ...
Hydrogel Contact Lens Dehydration in Controlled Environmental Conditions. -
PB Morgan, N Efron, SL Morgan, SA Little - Eye & Contact Lens: Science and Clinical Practice, 2004 - claojournal.org
... & Clinical Practice:Volume 30(2)April 2004pp 99-102. ... and after each session using
a soft contact lens refractometer ... or the two lens types (F 1 = 1.4, P = 0.29). ...
Source: Google Scholar |